Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2408 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2408 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component file E40654. 02408 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.47 %
0.47 %
ASTM D570
Linear Mold Shrinkage 0.0044 cm/cm
0.0044 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 87
87
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.68 %
0.68 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Compressive Strength 207 MPa
30000 psi
ASTM D695
Izod Impact, Notched 0.188 J/cm
0.352 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.188 J/cm²
0.895 ft-lb/in²
ASTM D256
Impact 122
122
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 40.0 - 130 °C
35.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 193 °C
379 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 27.6 %
27.6 %
ASTM D2863
Shrinkage 0.208 %
0.208 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+12 ohm-cm
1.20e+12 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 14.2 kV/mm
361 kV/in
Short Time; ASTM D149
Dissipation Factor 0.051
0.051
ASTM D150
Arc Resistance 136 sec
136 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638