Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 150 - 195 °C | 302 - 383 °F | Average value: 179 °C Grade Count:22 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 165 - 195 °C | 329 - 383 °F | Average value: 180 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 165 - 195 °C | 329 - 383 °F | Average value: 180 °C Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Maximum Service Temperature, Air | 165 - 195 °C | 329 - 383 °F | Average value: 180 °C Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |