Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 165 °C | 329 °F | Recommended |
Nye Lubricants 701 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | Continuous Use; UL-746B |
Gharda Chemicals Gafone S 1320GF Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | <20000 hours; IEC 60216-P1 |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20/AF/15/TF/10 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20/XCF/30 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7324 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7908 Polyphthalamide, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Maximum Service Temperature, Air | 165 - 175 °C | 329 - 347 °F | Softening Range |
Huntsman HT 9719-1 Aromatic Amine Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: 3,3' -diaminodiphenyl sulfone, micropulverized, solid amine. Composites, adhesives.Data provided by Ciba Speci.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Maximum Service Temperature, Air | 165 - 185 °C | 329 - 365 °F | Continuous Use |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | Heat Resistance; ASTM D570D |
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Maximum Service Temperature, Air | 165 °C @Time 10800 sec |
329 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6160 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Maximum Service Temperature, Air | 165 - 195 °C | 329 - 383 °F | Average value: 180 °C Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |