Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 1629 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 328 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 345 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 348 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 350 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 351 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 352 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 353 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 354 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 384 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 388 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 383 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 386 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | short excursions |
3M FG7-14 FB-700 Filter Bag Fabric 3M has developed a line of advanced textiles for manufacturing high temperature filter bags which can be used at temperatures up to 700°F (371°C), or for those even higher temperature applications.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | short excursions |
3M FG7-22 FB-700 Filter Bag Fabric 3M has developed a line of advanced textiles for manufacturing high temperature filter bags which can be used at temperatures up to 700°F (371°C), or for those even higher temperature applications.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | Intermittent |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | Creep is a concern above this temp |
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201 Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Maximum Service Temperature, Air | 427 °C | 801 °F | starts to carbonize |
Hexcel® HexForce™ 372 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Maximum Service Temperature, Air | 427 °C | 800 °F | |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |