Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sealabilityTemperature resistantNon-oxidizing fibersIFG® 5500 has passed the Garlock Fire Test and is ABS Fire Safe Type Approved.Media: Water, Aliphatic hydrocarbons, Oils, Gasoline, Saturated steam, Inert gases, Most refrigerantsInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0637 lb/in³
Permeability 0.050
0.050
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 10.3 MPa
1500 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 427 °C
800 °F
288 °C

@Pressure 8.27 MPa
550 °F

@Pressure 1200 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Strength 9.65 kV/mm

@Temperature 121 °C,
Time 10800 sec
245 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
11.2 kV/mm

@Temperature 121 °C,
Time 10800 sec
284 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
Descriptive Properties Value Comments
Color Gray
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 15
ASTM F38
Sealability ASTM F37B, ml/hr 0.2
ASTM Fuel A
1
Nitrogen
Users viewing this material also viewed the following: