Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 600 °C | 1110 °F | Continuous |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Oxidation Resistance |
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Sinotek Materials Packing Carbon Fiber with Graphite The packing is woven of strong carbon fiber after softening treatment and impregnation with the mixture of fine graphite powder, PTFE dispersion and lubricant. Being strong, static and heat-conducti.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si) Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fractu.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Good tensile and creep to 600°C |
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Continuous Use, with Glass Fiber Reinforcement |
Zircar Ceramics AS-1260 Alumina-Silica Textile Multiple forms of ceramic fiber textiles made of reinforced yarn. Amazingly strong, they are useful as gasketing, insulation and fire protection to temperatures of 1260°C (2300°F).Information pro.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Eifeler Coatings Technology CrCN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Eifeler Coatings Technology CrN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Elisto THERMOSTAR® LC 400 GL Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Operating Temperature |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M iM30K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K46 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Beijing Evergrow Resources GFF-10 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S22 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |