Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 760 °C | 1400 °F | Not recommended for use in continuous casting applications. |
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | Exception: Not recommended for use in continuous casting applications. |
Pyrotek Pyrocast AR FINE Castable Refractory Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | intermittent |
Pyrotek Pyrocast AR LITE Castable Refractory A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
Pyrotek T-20 Fiberglass Fabric Close woven fiberglass. Does not cause severe skin irritation. Lightweight, light-brown, chemical resistant fabric.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | Continuous |
Mid-Mountain Materials HYTEX® 1400 Fiberglass Industrial Textile Description: Hytex is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying che.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | <100 hr, depends on temperature gradient |
Schott ROBAX® Glass Ceramic ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | Used as a non-conducting structural component up to this temp. |
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
XADC-Armoloy Diamond-Chrome Composite Coating XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Fiberwall® 304 SS Systems Hardware The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | Significant oxidation resistance to this temp. |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
BNZ Materials 375 Insulating Cement 375 Finishing Cement is a one coat finish which hardens to a smooth, crack-free surface in a few hours. This surface may then be painted with a water-base paint. Recommended for insulating small ste.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 760 °C | 1400 °F | |
Aremco Pyro-Putty™ 1000 High Temperature Ceramic-Metallic Putty, Aluminum Filled Ceramic and Aluminum-Filled, Two-Part, Water Based Paste.For Applications to 1/2" Thick.Repairs Cast Aluminum Parts to 1400°F |