Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 116 °C @Load 1.00 kg |
241 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 116 °C @Load 1.00 kg |
241 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYplex PMMA 500 Acrylic Glass Information provided by Polykemi AB |
|||
Vicat Softening Point | 116 °C @Load 1.02 kg |
241 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Vicat Softening Point | 116 °C @Load 0.999 kg |
241 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |