Polykemi AB POLYplex PMMA 500 Acrylic Glass

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Polykemi AB
Trade Name POLYplex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYplex PMMA 500 Acrylic Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Melt Index of Compound 2.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 80.0 MPa
<= 11600 psi
ISO/R527
Elongation at Yield 10 %
10 %
ISO/R527
Flexural Strength <= 140 MPa
<= 20300 psi
ISO 178
Flexural Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
120°C/h; ISO 75/1
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
116 °C

@Load 1.00 kg
241 °F

@Load 2.21 lb
50°C/h; ISO 306