Polymer Property : Vicat Softening Point = 149 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 65.0 °C

@Load 5.10 kg
149 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact
Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati..
Vicat Softening Point 65.0 °C

@Load 5.10 kg
149 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com..
Vicat Softening Point 65.0 °C

@Load 5.10 kg
149 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive
Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag..
Vicat Softening Point 65.0 °C

@Load 5.10 kg
149 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i..