Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 192 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C

@Load 5.001 kg
192 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade
Information provided by Polykemi AB
Vicat Softening Point 89.0 °C

@Load 1.02 kg
192 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution PS 165 N/L GPPS
Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS..
Vicat Softening Point 89.0 °C

@Load 5.10 kg
192 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution PS 495N HIPS
Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor..
Vicat Softening Point 89.0 °C

@Load 5.10 kg
192 °F

@Load 11.2 lb
ISO 306
Borealis HK030U Polypropylene Compound
HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit..
Vicat Softening Point 89.0 °C

@Load 5.10 kg
192 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM..
Vicat Softening Point 89.0 °C

@Load 5.00 kg
192 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 0412 Polystyrene
Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 89.0 °C

@Load 5.00 kg
192 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene
Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 89.0 °C

@Load 1.00 kg
192 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibiton® PB-5910 SBC
High transparency, medium stiffness, toughness
Vicat Softening Point 89.0 °C

@Load 5.00 kg
192 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
High impact
Vicat Softening Point 89.0 °C

@Load 5.00 kg
192 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion
Extrusion
Vicat Softening Point 89.0 °C

@Load 5.00 kg
192 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PG-33 Polystyrene
Standard grade
Vicat Softening Point 89.0 °C

@Load 5.001 kg
192 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 89.0 °C

@Load 5.001 kg
192 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Copyright © lookpolymers.com All Rights Reserved