Polymer Property : Vicat Softening Point = 200 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B12^ NH9 Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B12^ NH9L Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B12^ Nylon 6
Information provided by Polykemi AB
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
120°C/h; ISO 306
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
50°C/h; ISO 306
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
120°C/hour; ISO 306
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
50°C/hour; ISO 306
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Vicat Softening Point >= 200 °C

@Load 5.10 kg
>= 392 °F

@Load 11.2 lb
120°C/h; ISO 306
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
Vicat Softening Point >= 200 °C

@Load 5.10 kg
>= 392 °F

@Load 11.2 lb
50°C/h; ISO 306
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
Vicat Softening Point >= 200 °C

@Load 5.10 kg
>= 392 °F

@Load 11.2 lb
120°C/hour; ISO 306
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Vicat Softening Point >= 200 °C

@Load 5.10 kg
>= 392 °F

@Load 11.2 lb
50°C/hour; ISO 306
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..