Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 40.0 °C @Load 5.10 kg |
104 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Vicat Softening Point | 40.0 °C @Load 5.10 kg |
104 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |