Vicat Softening Point 49.0 °C

@Load 5.10 kg
120 °F

@Load 11.2 lb
ISO 306
Borealis Daplen™ ED230HP Polypropylene TPO Compound
Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
Vicat Softening Point 49.0 °C

@Load 5.10 kg
120 °F

@Load 11.2 lb
ISO 306
Borealis Daplen™ EG250AI Polypropylene TPO Compound
Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv..