Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.0244 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0244 W/m-K

@Temperature 400 °C
0.169 BTU-in/hr-ft²-°F

@Temperature 752 °F
@ 320 kg/m³; ASTM C177, ISO 8302
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1”) upwards. F..
Copyright © lookpolymers.com All Rights Reserved