Polymer Property : Thermal Conductivity = 0.300 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.220 - 0.300 W/m-K

@Temperature 100 °C
1.53 - 2.08 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable
Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th..
Thermal Conductivity 0.200 - 0.300 W/m-K

@Temperature 100 °C
1.39 - 2.08 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable
Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati..
Thermal Conductivity 0.220 - 0.300 W/m-K

@Temperature 950 °C
1.53 - 2.08 BTU-in/hr-ft²-°F

@Temperature 1740 °F
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable
Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in..