Thermal Properties Metric English Comments
Thermal Conductivity 0.320 W/m-K

@Temperature 450 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 842 °F
Pyrotek Pyrotherm M-68 Structural Insulation Board
Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i..
Thermal Conductivity 0.320 W/m-K

@Temperature 260 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 500 °F
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to..
Thermal Conductivity 0.320 W/m-K

@Temperature 23.0 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Along flow; ISO 22007-4
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Thermal Conductivity 0.320 W/m-K

@Temperature 250 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM D1530
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Thermal Conductivity 0.320 W/m-K

@Temperature 250 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Thermal Conductivity 0.320 W/m-K

@Temperature 250 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Thermal Conductivity 0.320 W/m-K

@Temperature 100 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Thermal Conductivity 0.320 - 0.420 W/m-K

@Temperature 600 °C
2.22 - 2.91 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GI 28 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.320 - 0.420 W/m-K

@Temperature 100 °C
2.22 - 2.91 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable
Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al..
Thermal Conductivity 0.320 - 0.420 W/m-K

@Temperature 1000 °C
2.22 - 2.91 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable
Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast ..
Thermal Conductivity 0.320 W/m-K

@Temperature 900 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Zircar Refractory Composites RS-99-60 Refractory Sheet
ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani..
Thermal Conductivity 0.320 W/m-K

@Temperature 1600 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 2910 °F
parallel to thickness
Zircar Refractory Composites RS-3000 ALUMINA FELT
ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It..
Thermal Conductivity 0.320 W/m-K

@Temperature 538 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials BNZ-26 HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 816 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 1000 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials BNZP-23B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 600 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials BNZP-26 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 816 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials C-22 Z Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 800 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1470 °F
ASTM C182
BNZ Materials Color A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 400 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C182
BNZ Materials Color CA Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 W/m-K

@Temperature 816 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials PA 20 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.320 - 0.420 W/m-K

@Temperature 100 °C
2.22 - 2.91 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE MW Refractory Insulating Castable
Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al..