Thermal Properties Metric English Comments
Thermal Conductivity 0.0580 W/m-K

@Temperature 200 °C
0.403 BTU-in/hr-ft²-°F

@Temperature 392 °F
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
Microtherm Group MT Thermosphere® Moldable Insulation Paste
MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste..
Thermal Conductivity 0.0580 W/m-K

@Temperature 80.0 °C
0.403 BTU-in/hr-ft²-°F

@Temperature 176 °F
3M Novec™ 7500 Engineered Fluid
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a..