Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.460 - 0.560 W/m-K @Temperature 1370 °C |
3.19 - 3.89 BTU-in/hr-ft²-°F @Temperature 2500 °F |
|
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:.. |
|||
Thermal Conductivity | 0.460 - 0.560 W/m-K @Temperature 1370 °C |
3.19 - 3.89 BTU-in/hr-ft²-°F @Temperature 2500 °F |
|
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |