Polymer Property : Thermal Conductivity = 0.790 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.790 W/m-K

@Temperature 400 °C
5.48 BTU-in/hr-ft²-°F

@Temperature 752 °F
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..
Thermal Conductivity 0.790 - 0.890 W/m-K

@Temperature 1300 °C
5.48 - 6.18 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 165 Dense Refractory Castable
Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa..