Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 P Moldable Refractory Material Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. .. |
|||
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Thermal Conductivity | 0.890 - 1.09 W/m-K @Temperature 1300 °C |
6.18 - 7.56 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin.. |
|||
Thermal Conductivity | 0.890 - 1.09 W/m-K @Temperature 1000 °C |
6.18 - 7.56 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |