Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.890 - 0.990 W/m-K

@Temperature 100 °C
6.18 - 6.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 85 P Moldable Refractory Material
Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. ..
Thermal Conductivity 0.890 - 0.990 W/m-K

@Temperature 100 °C
6.18 - 6.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go..
Thermal Conductivity 0.890 - 1.09 W/m-K

@Temperature 1300 °C
6.18 - 7.56 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable
Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va..
Thermal Conductivity 0.890 - 0.990 W/m-K

@Temperature 100 °C
6.18 - 6.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material
Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin..
Thermal Conductivity 0.890 - 1.09 W/m-K

@Temperature 1000 °C
6.18 - 7.56 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GI 34 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.