Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.08 W/m-K @Temperature 550 °C |
7.50 BTU-in/hr-ft²-°F @Temperature 1020 °F |
|
Pyrotek Pyrocast 220HT Refractory Castable Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r.. |