Thermal Properties Metric English Comments
Thermal Conductivity 1.08 W/m-K

@Temperature 550 °C
7.50 BTU-in/hr-ft²-°F

@Temperature 1020 °F
Pyrotek Pyrocast 220HT Refractory Castable
Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r..