Polymer Property : Thermal Conductivity = 1.30 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.30 W/m-K

@Temperature 650 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 42 Dense Refractory Brick
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c..
Thermal Conductivity 1.30 W/m-K

@Temperature 100 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 46 S Dense Refractory Brick
Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%..
Thermal Conductivity 1.30 W/m-K

@Temperature 100 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 50 Dense Refractory Brick
Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato..
Thermal Conductivity 1.30 W/m-K

@Temperature 650 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast A 1 S Dense Refractory Brick
Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai..
Thermal Conductivity 1.30 W/m-K

@Temperature 1100 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast C Sp Dense Refractory Brick
Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.30 W/m-K

@Temperature 900 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 1650 °F
EN 993-15 199
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick
Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con..