Gouda Vuurvast AK 42 Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 42 Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.25 g/cc
0.0813 lb/in³
Apparent
Porosity 15 %
15 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.20 W/m-K

@Temperature 100 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.30 W/m-K

@Temperature 650 °C
9.02 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.45 W/m-K

@Temperature 1100 °C
10.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
1500 °C
2730 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 42 %
42 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 53 %
53 %
Descriptive Properties Value Comments
Segercone 34-35
Thermal Shock Resistance 15 cycles
DIN 51068