Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.65 - 1.85 W/m-K @Temperature 100 °C |
11.5 - 12.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Thermal Conductivity | 1.65 - 1.85 W/m-K @Temperature 600 °C |
11.5 - 12.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Thermal Conductivity | 1.65 - 1.85 W/m-K @Temperature 100 °C |
11.5 - 12.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Thermal Conductivity | 1.65 - 1.85 W/m-K @Temperature 600 °C |
11.5 - 12.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Thermal Conductivity | 1.66 W/m-K @Temperature 538 °C |
11.5 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable Pyrocast ALF3 is a low cement castable with a high-purity mullite base. It is suited for applications exposed to high erosion or aggressive alloys and/or atmospheres.ApplicationsAluminum melting an.. |