Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name VIBRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
100 - 120 MPa

@Temperature 1300 °C
14500 - 17400 psi

@Temperature 2370 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.65 - 1.85 W/m-K

@Temperature 100 °C
11.5 - 12.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.65 - 1.85 W/m-K

@Temperature 600 °C
11.5 - 12.8 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.70 - 1.90 W/m-K

@Temperature 1300 °C
11.8 - 13.2 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1300 °C
-0.200 - 0.200 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 75 %
75 %
Fe2O3 1.0 %
1.0 %
SiO2 8.0 %
8.0 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2750 kg
Mixing Water 4.5-5 liters
per 100 kgs dry material