Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 65% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 316 °C |
118 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 200 °C |
118 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |