Assab Steels VANADIS 10 Cold Work Steel

Category Metal , Ferrous Metal , Chrome-moly Steel , Tool Steel , Cold Work Steel
Manufacturer Assab Steels
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Assab Steels VANADIS 10 Cold Work Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughnessVery good stability in hardeningGood resistance to tempering backGood MachinabilitySimple heat treatmentSuitable for surface treatmentVANADIS 4 is especially suitable for very long run tooling where adhesive wear is the dominating problem. Its very good combination of extremely high wear resistance and toughness also make VANADIS 10 an interesting alternative in applications where tooling made of such materials as cemented carbide tends to chip or crack.Examples:Blanking and formingFine blankingBlanking of electrical sheetGasket stampingDeep drawingCold ForgingSlitting knives (paper and foil)Powder pressingGranulator knivesExtruder screws, etc
Physical Properties Metric English Comments
Density 7.42 g/cc
0.268 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58
58
1020°C Austenitizing temperature, for tempering at 550°C
60
60
1060°C Austenitizing temperature, for tempering at 550°C
62
62
Hardened and tempered.
62
62
1020°C Austenitizing temperature, for tempering at 300°C
63
63
1020°C Austenitizing temperature, for tempering at 500°C
63
63
1060°C Austenitizing temperature, for tempering at 300°C
64
64
Holding time 30 minutes, Air cooling, 1000°C Austenitizing temperature
65
65
1060°C Austenitizing temperature, for tempering at 500°C
66
66
Holding time 30 minutes, Air cooling, 1050°C Austenitizing temperature
Modulus of Elasticity 234 GPa
33900 ksi
Impact Test 17.5 J
12.9 ft-lb
tempering temperature of 475°C. Specimen size: 7x10x55 mm unnotched. Hardened at 1020°C. Quenched in air. Tempered twice
22.5 J
16.6 ft-lb
tempering temperature of 275°C. Specimen size: 7x10x55 mm unnotched. Hardened at 1020°C. Quenched in air. Tempered twice
27.5 J
20.3 ft-lb
tempering temperature of 575°C. Specimen size: 7x10x55 mm unnotched. Hardened at 1020°C. Quenched in air. Tempered twice
Thermal Properties Metric English Comments
CTE, linear 10.9 µm/m-°C

@Temperature 20.0 - 200 °C
6.06 µin/in-°F

@Temperature 68.0 - 392 °F
11.7 µm/m-°C

@Temperature 20.0 - 400 °C
6.50 µin/in-°F

@Temperature 68.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 14.0 W/m-K

@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
17.0 W/m-K

@Temperature 200 °C
118 BTU-in/hr-ft²-°F

@Temperature 392 °F
19.0 W/m-K

@Temperature 400 °C
132 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 2.9 %
2.9 %
Chromium, Cr 8.0 %
8.0 %
Iron, Fe 76.3 %
76.3 %
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 1.5 %
1.5 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 9.8 %
9.8 %