Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.3 W/m-K @Temperature 500 °C |
113 BTU-in/hr-ft²-°F @Temperature 932 °F |
Hardened Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 10% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 0% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |