Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.30 - 2.40 W/m-K @Temperature 100 °C |
16.0 - 16.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 Moldable Refractory Material Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an.. |