Polymer Property : Thermal Conductivity = 191 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 27.5 W/m-K

@Temperature 200 °C
191 BTU-in/hr-ft²-°F

@Temperature 392 °F
International Mold Steel DH31-EX Die Cast & Forging Steel
DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b..
Thermal Conductivity 27.5 W/m-K

@Temperature 700 °C
191 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Latrobe LSSâ„¢ 2367 Hot Work Tool Steel
TLS 2367 is a chromium-molybdenum hot work steel that is similar to AISI H11 hot work steel, but which contains a higher molybdenum content. The higher molybdenum gives TLS 2367 better hot hardness ..
Thermal Conductivity 27.5 W/m-K

@Temperature 343 °C
191 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel
Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re..
Thermal Conductivity 27.5 W/m-K

@Temperature 600 °C
191 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Hardened and Tempered
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..
Thermal Conductivity 27.5 W/m-K

@Temperature 343 °C
191 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel
Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a..