Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, mill annealed HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 50% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, Annealed (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 30% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 10% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |