Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 35.0 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 35.0 W/m-K

@Temperature 700 °C
243 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Latrobe LSSâ„¢ 2714 Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714 is a nickel-chromium-molybdenum hot work steel that exhibits high impact toughness and good resistance to softening at elevated temperature. The high nickel content imparts the toughness as..
Thermal Conductivity 35.0 W/m-K

@Temperature 700 °C
243 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Latrobe LSSâ„¢ 2714T Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714HT is the same steel available from inventory in a heat-treated condition, at a hardness of 352 to 401 HBS (approximately 38 to 43 HRC). TLS 2714HT can be readily flame cut, and this propert..