Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.520 - 0.620 W/m-K @Temperature 600 °C |
3.61 - 4.30 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Thermal Conductivity | 0.520 - 0.620 W/m-K @Temperature 100 °C |
3.61 - 4.30 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan.. |