Thermal Properties Metric English Comments
Thermal Conductivity 0.630 - 0.730 W/m-K

@Temperature 1000 °C
4.37 - 5.07 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Thermal Conductivity 0.630 - 0.730 W/m-K

@Temperature 100 °C
4.37 - 5.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..