Material Notes:
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 20.0 - 30.0 MPa

@Temperature 1300 °C
2900 - 4350 psi

@Temperature 2370 °F
Cold Crushing Strength
35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.630 - 0.730 W/m-K

@Temperature 100 °C
4.37 - 5.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.700 - 0.800 W/m-K

@Temperature 600 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.810 - 0.910 W/m-K

@Temperature 1300 °C
5.62 - 6.32 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage -1.50 - 1.50 %

@Temperature 1300 °C
-1.50 - 1.50 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 62 %
62 %
Fe2O3 1.5 %
1.5 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2300 kg