Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.700 - 0.800 W/m-K @Temperature 100 °C |
4.86 - 5.55 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Thermal Conductivity | 0.700 - 0.900 W/m-K @Temperature 100 °C |
4.86 - 6.25 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Thermal Conductivity | 0.700 - 0.800 W/m-K @Temperature 100 °C |
4.86 - 5.55 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 40 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl.. |
|||
Thermal Conductivity | 0.700 - 0.800 W/m-K @Temperature 100 °C |
4.86 - 5.55 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Thermal Conductivity | 0.700 - 0.800 W/m-K @Temperature 100 °C |
4.86 - 5.55 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 50 D Moldable Refractory Material Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the.. |
|||
Thermal Conductivity | 0.700 - 0.800 W/m-K @Temperature 600 °C |
4.86 - 5.55 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 165 GM Dense Refractory Castable Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 500 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Touchstone CFOAM® 20 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |