Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.610 - 0.710 W/m-K @Temperature 600 °C |
4.23 - 4.93 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.610 - 0.710 W/m-K @Temperature 100 °C |
4.23 - 4.93 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Thermal Conductivity | 0.610 - 0.710 W/m-K @Temperature 100 °C |
4.23 - 4.93 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Thermal Conductivity | 0.610 - 0.710 W/m-K @Temperature 100 °C |
4.23 - 4.93 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |
|||
Thermal Conductivity | 0.610 - 0.710 W/m-K @Temperature 100 °C |
4.23 - 4.93 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 165 Dense Refractory Castable Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa.. |