Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.820 W/m-K @Temperature 700 °C |
5.69 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Thermal Conductivity | 0.820 W/m-K @Temperature 700 °C |
5.69 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast AR FINE Castable Refractory Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting.. |
|||
Thermal Conductivity | 0.820 W/m-K @Temperature 815 °C |
5.69 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek Pyrocast ICL Castable Refractory Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist.. |
|||
Thermal Conductivity | 0.820 - 0.920 W/m-K @Temperature 600 °C |
5.69 - 6.38 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.820 - 0.920 W/m-K @Temperature 600 °C |
5.69 - 6.38 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Thermal Conductivity | 0.820 - 0.920 W/m-K @Temperature 1400 °C |
5.69 - 6.38 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Thermal Conductivity | 0.820 - 0.920 W/m-K @Temperature 600 °C |
5.69 - 6.38 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |