Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 157 °C | 315 °F | |
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Solidus | 157 °C | 315 °F | |
Williams Advanced Alloys WS157 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |