Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 197 °C | 387 °F | |
Indium Corp. Indalloy® 206 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |