Material Notes:
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 9.30 g/cc
0.336 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 19.0 W/m-K

@Temperature 85.0 °C
132 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 197 - 231 °C
387 - 448 °F
Solidus 197 °C
387 °F
Liquidus 231 °C
448 °F
Component Elements Properties Metric English Comments
Indium, In 40 %
40 %
Lead, Pb 60 %
60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000330 ohm-cm
0.0000330 ohm-cm