Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 950.0 °C | 1742 °F | Melting Point |
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy Applications:Premabraze 130 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |
|||
Solidus | 950.0 °C | 1742 °F | Melting Point |
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy Applications:Premabraze 131 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s.. |
|||
Solidus | 950.0 °C | 1742 °F | |
Universal Wire Works BAu-4 (AMS 4787) Gold Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |