Universal Wire Works BAu-4 (AMS 4787) Gold Brazing Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works BAu-4 (AMS 4787) Gold Brazing Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Thermal Properties Metric English Comments
Melting Point 950.0 - 950.0 °C
1742 - 1742 °F
Solidus 950.0 °C
1742 °F
Liquidus 950.0 °C
1742 °F
Component Elements Properties Metric English Comments
Gold, Au 82 %
82 %
Nickel, Ni 18 %
18 %