Polymer Property : Liquidus = 1260 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1260 °C
2300 °F
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Liquidus 1260 °C
2300 °F
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Liquidus 1260 °C
2300 °F
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Liquidus 1260 °C
2300 °F
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Liquidus 1260 °C
2300 °F
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Liquidus 1260 °C
2300 °F
Weartech International WT-1 Cobalt Hardfacing & Wear Resistant Alloy
Applications: seaming rolls, valve seats, wear pads, pump sleeves, seals, bearings, bushings, saw blades, cuttersInformation provided by Weartech International
Liquidus 1260 °C
2300 °F
Weartech International WT-20 Cobalt Hardfacing & Wear Resistant Alloy
Applications: marine engine valves, control valves for petrochemicals, steel mill rolls, homogenizer valve componentsInformation provided by Weartech International
Liquidus 1260 °C
2300 °F
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy
Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness ..