Polymer Property : Liquidus = 1308 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1308 °C
2386 °F
Kennametal Stellite Delcrome® 90
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and..