Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Delcrome® 90

Category Metal , Ferrous Metal , Cast Iron , Alloy Cast Iron , White Cast Iron
Manufacturer Kennametal Stellite
Trade Name Delcrome®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Delcrome® 90.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and improved corrosion resistance.Processing: Anneal: 6hours/790°C (1450°F), furnace cool to HRC 35-45; Harden: 2 hours/1090°C (1980°F), air cooled to HRC 55-63. Can be milled and turned in the annealed condition if hardness is below HRC 40. Final grinding should be done on hardened piece to allow for distortion during heat treatment.Corrosion Resistance: Generally superior to mild steel, but worse than 410 stainless steel. Significant corrosion in weak acids and will pit in the presence of chloride. Oxidation resistance up to 980°C (1800°F).Applications: Abrasive applications below 540°C (1000°F) where corrosion is mild; pulverizer parts, pump barrel liners, cement valve slides, wear plates, and dry bearings.Forms: Shapes using all casting processes, comparable hardfacing consumables.Product of former Deloro Stellite Inc. Similar to Delcrome 50V
Physical Properties Metric English Comments
Density 7.59 g/cc
0.274 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 595 - 740
595 - 740
70

@Temperature 900 °C
70

@Temperature 1650 °F
Hot Hardness
164

@Temperature 700 °C
164

@Temperature 1290 °F
Hot Hardness
228

@Temperature 600 °C
228

@Temperature 1110 °F
Hot Hardness
338

@Temperature 500 °C
338

@Temperature 932 °F
Hot Hardness
400

@Temperature 400 °C
400

@Temperature 752 °F
Hot Hardness
540

@Temperature 20.0 °C
540

@Temperature 68.0 °F
Hot Hardness
Hardness, Knoop 667 - 830
667 - 830
Converted from Brinell hardness
Hardness, Rockwell C 55 - 63
55 - 63
Hardness, Vickers 640 - 798
640 - 798
Converted from Brinell hardness.
Tensile Strength, Ultimate 450 MPa
65300 psi
Elongation at Break <= 1.0 %
<= 1.0 %
Modulus of Elasticity 225 GPa
32600 ksi
Izod Impact Unnotched 4.00 J
2.95 ft-lb
Thermal Properties Metric English Comments
CTE, linear 12.03 µm/m-°C

@Temperature 20.0 - 100 °C
6.683 µin/in-°F

@Temperature 68.0 - 212 °F
14.46 µm/m-°C

@Temperature 20.0 - 300 °C
8.033 µin/in-°F

@Temperature 68.0 - 572 °F
15.18 µm/m-°C

@Temperature 20.0 - 900 °C
8.433 µin/in-°F

@Temperature 68.0 - 1650 °F
15.72 µm/m-°C

@Temperature 20.0 - 700 °C
8.733 µin/in-°F

@Temperature 68.0 - 1290 °F
15.73 µm/m-°C

@Temperature 20.0 - 500 °C
8.739 µin/in-°F

@Temperature 68.0 - 932 °F
Melting Point 1255 - 1308 °C
2291 - 2386 °F
Solidus 1255 °C
2291 °F
Liquidus 1308 °C
2386 °F
Component Elements Properties Metric English Comments
Carbon, C 2.7 %
2.7 %
Chromium, Cr 27 %
27 %
Iron, Fe 67.8 %
67.8 %
Manganese, Mn 0.90 %
0.90 %
Silicon, Si 0.80 %
0.80 %
Vanadium, V 0.80 %
0.80 %
Users viewing this material also viewed the following: