Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 143 °C | 289 °F | |
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 143 °C | 289 °F | |
Indium Corp. Indalloy® 290 In-Ag Solder Alloy Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,.. |
|||
Liquidus | 143 °C | 289 °F | |
Williams Advanced Alloys WS143 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |